现货医疗器械/PC/PET 美国基础创新 X8300MR BK1D168
PC/PET塑料加工工艺
干燥时间4.0到6.0 hr,干燥时间,大36 hr,建议的大水分含量0.010 %,螺筒后部温度243到254 °C,螺筒中部温度246到257 °C,螺筒前部温度249到260 °C,射嘴温度252到263 °C,加工(熔体)温度260到274 °C,模具温度18.3到65.6 °C,注塑温度68.9到138 MPa,注射速度中等偏慢。PC/PET具体加工参数视改性成分而定,
用途 | Water Management草坪和园林设备电气/电子应用领域电气元件电器用具电子显示器光学应用室外应用医疗/护理用品医疗器械照明应用 |
多点数据 | Coefficient of Thermal Expansion vs. Temperature (ASTM E831) Flexural DMA (ASTM D4065) Shear DMA (ASTM D4065) Specific Heat vs. Temperature (ASTM D3417) Tensile Stress vs. Strain (ASTM D638) Thermal Conductivity vs. Temperature (ASTM E1530) Viscosity vs. Shear Rate (ASTM D3835) |
Also Available In | Asia PacificEurope |